Tubalan Zirconia

Kyakkyawan aikin ado fiye da farin zirconia.
Bibiyar VITA sosai® Jagoran Inuwa Classic.
Ana amfani da cikakken baka da gada mai tsayi.


Bloomden® 3D Pro multilayer zirconia ba kamar kowane zirconia ba, yana iya nuna ƙarfin ƙarfi daga 800MPa zuwa 1200MPa wanda zai iya rufe baya da gabaɗaya don duka rawanin da gadoji gami da gyare-gyaren dasa.

Muna ba da madaidaicin launi don VITA® Cikakken kewayon inuwa 16, gami da BL2. Ingancin mu yana daidai da batches, kuma masu fasahar hakori a duka Turai da Amurka sun tabbatar da daidaiton launi na mu.

Bloomden farin zirconia kyakkyawan sakamako na masking. yana iya yin tasiri yadda ya kamata ya rufe abubuwan da suka canza launin ko tabo masu duhu, yana haifar da kyan gani mai kyau. Wannan yana da mahimmanci musamman ga marasa lafiya waɗanda suka san kansu game da murmushinsu ko kuma suna son maidowa wanda yayi kama da na halitta kamar yadda zai yiwu.
Ana samun sabuntawa tare da cikakken rawanin kwane-kwane, gadoji, veneers ko cikakken baka.

Maimaitawa

Kambi na gaba

Kambi na baya

Inlay

Full Crown Bridge

Kambi mai mahimmanci

Zuba cikakken Arch

Cikakken baka gada
| Technical dalla | |||
| Cubic-C |
Muhimmancin-C |
M-C |
|
| Zr02+ HfO2+Y203 | ≥98% | ≥98% | ≥98% |
| Y203 | 8% -10% | 5.5% -8.0% | 4.5% -6.0% |
| AI203 | <0.5% | <0.15% | <0.5% |
| Yawawa Kafin Tsayawa (g.cm-3) | 3.20 ± 0.05 | 3.15 ± 0.05 | 3.15 ± 0.05 |
| Girman Bayan Sintering (g.cm-3) | 6.06 ± 0.01 | 6.08 ± 0.01 | 6.09 ± 0.01 |
| CTE (25-500 ℃) (K-1) | 10.0 ± 0.5% | 10.5 ± 0.5% | 10.5 ± 0.5% |
| Ƙarfin Flexural Bayan Sintering (MPa) | > 600 | > 900 | > 1100 |
| Tsufa Surface Monoclinic Matakin Abun ciki | <15% | <15% | <15% |
| Canji | <49% | <46% | <43% |
| Solubility Bayan Sintering (ug.cm-2) | |||
| Cytotoxicity | Matsayi na 0 | Matsayi na 0 | Matsayi na 0 |
| Radioactivity (Bq.g-1)) | |||
| Zazzabi (℃) | 1450 | 1530 | 1530 |
| Systems | 98mm/95mm/92*75mm | ||
| kauri | 12m/14mm/16mm/18mm/20mm/22mm/25mm | ||
| Inuwa | A1 A2 A3 A3.5 A4/B1 B2 B3 B4/C1 C2 C3 C4/D2 D3 D4 | ||


Na kasance ina amfani da fasahar sintering mai sauri na zirconia tsawon watanni da yawa yanzu, kuma na yi farin ciki da sakamakon. Tsarin ɓacin rai da sauri ya rage yawan lokacin da ake ɗauka don samar da ingantaccen gyaran gyare-gyare na zirconia, yana ba ni damar ɗaukar ƙarin aiki da haɓaka yawan aiki na. Ƙarfi da ƙaya na gyare-gyare suna da kyau, idan ba mafi kyau ba, fiye da hanyoyin yin amfani da su na gargajiya, kuma marasa lafiya na sun gamsu da sakamakon. Ina godiya da rage yawan amfani da makamashi, wanda ke sa tsarin ya fi dacewa da muhalli.