Tubalan Zirconia

Bloomden multilayer zirconia yana ba da ƙarin haske na halitta, wanda ya ba shi damar haɗuwa da juna tare da haƙoran da ke kewaye, yana mai da shi kyakkyawan zaɓi don sabuntawa.
Multilayer zirconia yana da jituwa, ma'ana yana dacewa da jikin mutum, yana haifar da rashin lahani ko rashin lafiya.
Multilayer zirconia prosthetic kayan don CAD/CAM ta masu fasaha kuma sun ba da hangen nesa mai ban mamaki ga hakori.

Me yasa zabar Bloomden Multilayer Zirconia?

Ana samun sabuntawa tare da cikakken rawanin kwane-kwane, gadoji, veneers ko cikakken baka.

Maimaitawa

Kambi na gaba

Kambi na baya

Inlay

Full Crown Bridge

Kambi mai mahimmanci

Zuba Cikakken Arch

Cikakken Arch Bridge
| Cubic-ML | Muhimmancin-ML | M-ML | |
| ZrO2+HfO2+Y203 | ≥98% | ≥98% | ≥98% |
| Y203 | 8% -10% | 5.5% -8.0% | 4.5% -6.0% |
| Yawan yawa kafin Sintering (g.cm-3) | 3.20 ± 0.05 | 3.15 ± 0.05 | 3.15 ± 0.05 |
| Yawa bayan Sintering (g.cm-3) | 6.06 ± 0.01 | 6.08 ± 0.01 | 6.09 ± 0.01 |
| CTE (25-500 ℃) (K-1) | 10.0 ± 0.5 | 10.5 ± 0.5 | 10.5 ± 0.5 |
| Ƙarfin Flexural Bayan Sintering (MPa) | > 600 | > 900 | > 1100 |
| Tsufa Surface Monoclinic Matakin Abun ciki | <15% | <15% | <15% |
| Canji | <49% | <46% | <43% |
| Solubility Bayan Sintering (ug.cm-2) | |||
| Cytotoxicity | Matsayi na 0 | Matsayi na 0 | Matsayi na 0 |
| Radiyoactivity (Bq.g-1) | |||
| Zazzabi (℃) | 1450 | 1530 | 1530 |
| Systems | 98mm/95mm/92*75mm | ||
| kauri | 12m/14mm/16mm/18mm/20mm/22mm/25mm | ||
| Inuwa | A1 A2 A3 A3.5 A4/B1 B2 B3 B4/C1 C2 C3 C4/D2 D3 D4/ (BL1 BL2 BL3 BL4) | ||


Na kasance ina amfani da fasahar sintering mai sauri na zirconia tsawon watanni da yawa yanzu, kuma na yi farin ciki da sakamakon. Tsarin ɓacin rai da sauri ya rage yawan lokacin da ake ɗauka don samar da ingantaccen gyaran gyare-gyare na zirconia, yana ba ni damar ɗaukar ƙarin aiki da haɓaka yawan aiki na. Ƙarfi da ƙaya na gyare-gyare suna da kyau, idan ba mafi kyau ba, fiye da hanyoyin yin amfani da su na gargajiya, kuma marasa lafiya na sun gamsu da sakamakon. Ina godiya da rage yawan amfani da makamashi, wanda ke sa tsarin ya fi dacewa da muhalli.
Gabaɗaya, fasahar sintering mai sauri ta zirconia ta kasance mai canza wasa don ɗakin bincikena, kuma zan ba da shawarar sosai ga kowane ƙwararren hakori da ke neman haɓaka aikinsu da ingancin fitarwa.
Dr. Nathan Graves